ABS A310 北京[分类 牌号 厂家] 中间用空格键
| 规格级别 | 其它 其它 吹塑,挤出 | 外观颜色 | |
| 该料用途 | 医疗/保健应用、包装、油管 | ||
| 备注说明 | |||
| 性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | ||
| 物理性能 |
密度 | ASTM D-1505 | 0.934 | g/cm3 | ||
| 熔体流动速率 | 190℃/2.16kg | ASTM D-1238 | 3 | g/10min | ||
| VA含量 | 12 | wt% | ||||
| 热性能 | 熔点 | DSC | 97 | ℃ | ||
| 脆化温度 | ASTM D-1746 | -85 | ℃ | |||
| 维卡软化温度 | ASTM D-1525 | 75 | ℃ | |||
| 光学性能 |
光泽度 | 45°,75 µm | ASTM D-2457 | 38 | ||
| 雾度 | 75 µm | ASTM D-1003 | 13 | % | ||
| 机械性能 |
硬度 | Shore A | ASTM D-2240 | 95 | ||
| 硬度 | Shore D | ASTM D-2240 | 42 | |||
| 拉伸断裂强度 | ASTM D-638 | 16 | MPa | |||
| 断裂伸长率 | ASTM D-638 | 730 | % | |||
| 1%正割模量 | ASTM D-790 | 82 | MPa | |||
| 落锤冲击 | 25 µm | ASTM D-1709 | 70 | g | ||
| 拉伸屈服强度 | MD | 75 µm | ASTM D-882A | 7 | MPa | |
| TD | 6 | |||||
| 拉伸断裂强度 | MD | 75 µm | ASTM D-882A | 21 | MPa | |
| TD | 20 | |||||
| 断裂伸长率 | MD | 75 µm | ASTM D-882A | 460 | % | |
| TD | 560 | |||||