| 性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | 
            
                | 物理性能 | 密度 |  | ASTMD1505 | 0.921 | g/cm³ | 
            
                | 物理性能 | 熔流率(熔体流动速率) |  | ASTMD1238 | 2.5 | g/10min | 
            
                | 薄膜 | 薄膜厚度-经测试 |  |  | 38 | µm | 
            
                | 薄膜 | SecantModulus-1%Secant,MD(38µm,BlownFilm) |  | ASTMD882 | 186 | MPa | 
            
                | 薄膜 | SecantModulus-1%Secant,TD(38µm,BlownFilm) |  | ASTMD882 | 220 | MPa | 
            
                | 薄膜 | TensileStrength-MD(Break,38µm,CastFilm) |  | ASTMD882 | 26.0 | MPa | 
            
                | 薄膜 | TensileStrength-TD(Break,38µm,BlownFilm) |  | ASTMD882 | 19.0 | MPa | 
            
                | 薄膜 | TensileElongation-MD(Break,38µm,BlownFilm) |  | ASTMD882 | 250 | % | 
            
                | 薄膜 | TensileElongation-TD(Break,38µm,BlownFilm) |  | ASTMD882 | 750 | % | 
            
                | 薄膜 | 落锤冲击(38µm,吹塑薄膜) |  | ASTMD1709A | 100 | g | 
            
                | 光学性能 | 光泽度(45°,38.0µm,吹塑薄膜) |  | ASTMD2457 | 70 |  | 
            
                | 光学性能 | Haze(38.1µm,BlownFilm) |  | ASTMD1003 | 6.0 | % |