性能项目 |
试验条件[状态] |
测试方法 |
测试数据 |
数据单位 |
物理性能 |
密度 |
|
ASTMD1505 |
0.956 |
g/cm³ |
物理性能 |
熔流率(熔体流动速率)(190°C/2.16kg) |
|
ASTMD1238 |
0.80 |
g/10min |
薄膜 |
薄膜厚度-经测试 |
|
|
31 |
µm |
薄膜 |
可供应的薄膜厚度 |
|
|
Minimum12µm(0.5mil) |
|
薄膜 |
SecantModulus-1%Secant,MD(31µm,BlownFilm) |
|
ASTMD882 |
860 |
MPa |
薄膜 |
SecantModulus-1%Secant,TD(31µm,BlownFilm) |
|
ASTMD882 |
1040 |
MPa |
薄膜 |
抗张强度-MD(屈服,30µm,吹塑薄膜) |
|
ASTMD882 |
24.0 |
MPa |
薄膜 |
TensileStrength-TD(Yield,31µm,BlownFilm) |
|
ASTMD882 |
14.0 |
MPa |
薄膜 |
TensileStrength-MD(Break,31µm,BlownFilm) |
|
ASTMD882 |
52.0 |
MPa |
薄膜 |
TensileStrength-TD(Break,31µm,BlownFilm) |
|
ASTMD882 |
19.0 |
MPa |
薄膜 |
TensileElongation-MD(Break,31µm,BlownFilm) |
|
ASTMD882 |
570 |
% |
薄膜 |
TensileElongation-TD(Break,31µm,BlownFilm) |
|
ASTMD882 |
490 |
% |
薄膜 |
DartDropImpact2(31µm,BlownFilm) |
|
ASTMD1709A |
75 |
g |
薄膜 |
ElmendorfTearStrength-MD(31µm,BlownFilm) |
|
ASTMD1922 |
15 |
g |
薄膜 |
ElmendorfTearStrength-TD(31µm,BlownFilm) |
|
ASTMD1922 |
560 |
g |
热性能 |
熔融峰值温度 |
|
ASTMD3417 |
130 |
°C |